Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 44.0 MPa
6380 psi
ISO METHOD 176
NYCOA 2061 Copolymer Nylon 6/69
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Nylene® 452 Nylon 6
Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec..
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Kleerdex Kydex® GND Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Conductive fire-rated sheetApplications: Electronic equipment where protection against electro-static damage is essential, conductive floor mats, IC containers like trays, storage bins, boxes, chip ..
Flexural Yield Strength 44.0 - 76.0 MPa
6380 - 11000 psi
Average value: 66.1 MPa Grade Count:34
Overview of materials for PVC/Acrylic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate ..
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc..
Flexural Yield Strength 44.0 MPa
6380 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
Flexural Yield Strength 44.0 MPa
6380 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
Flexural Yield Strength 44.0 MPa
6380 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS
LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic.
Flexural Yield Strength 44.0 MPa
6380 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Tipco Tipcolene® FPC 30 - 30% Calcium Carbonate Reinforced Polypropylene Homopolymer
30% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Tipco Tipcolene® FPT 10 - 10% Talc Reinforced Polypropylene Homopolymer
10% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Tipco Tipcolene® FPT 20 FR VO LTHA - UL94-V0 Flame Retardant, 20% Talc Polypropylene Homopolymer, Long Term Heat Stability
20% Talc Reinforced PP Homopolymer with Long Term Heat StabilityApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., Ind..
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Washington Penn PPC3MF1.5-Black Polypropylene, 15% Mica-Filled, Chemically-Coupled
Heat Stabilized injection molding compound. Meets physical requirements for General Motors Spec. GMP.PP.024.Applications: HVAC duct and other various automotive applications.Data provided by Washin..
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Chevron Phillips K-Resin® KR01 Styrene-Butadiene Copolymer, Injection Molding Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC can be processed by injection molding and extrusion into attractive useful parts that have excellent clarity, good toughness, good stiffness, h..
Flexural Yield Strength 44.0 MPa
6380 psi
2 mm/min; ISO 178
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding
Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar.