Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 134 MPa | 19500 psi | ASTM D790 |
NYCOA 2037 15% Glass Filled Nylon 6 15% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS (Asia Pacific) |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Flexural Yield Strength | 134 - 185 MPa | 19500 - 26800 psi | Average value: 156 MPa Grade Count:15 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | ASTM D790 |
Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-sanitary products, electrical partsInformation provided b.. |
|||
Flexural Yield Strength | 134 MPa | 19500 psi | ASTM D790 |
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Flexural Yield Strength | 134 MPa | 19500 psi | ASTM D790 |
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC 11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East) LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Yield Strength | 134 MPa | 19400 psi | at 5% strain; ASTM D790 |
Covestro Makrolon® 8325 Polycarbonate High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
Flexural Yield Strength | 134 - 140 MPa @Temperature 80.0 - 80.0 °C |
19400 - 20300 psi @Temperature 176 - 176 °F |
Average value: 137 MPa Grade Count:4 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |
|||
Flexural Yield Strength | 134 MPa | 19500 psi | ASTM D790 |
PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |