Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the .. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 U represents the version of Flexirene FG 20 U.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
Iran Petrochemical (PCC) Arak 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Film Tensile Strength at Break, TD | 33.0 - 39.0 MPa | 4790 - 5660 psi | Average value: 36.7 MPa Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ISO 527-3 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ISO 527-3 |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip .. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | Cast Film at 1.25 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | |
Bapolene® 350F Polyethylene, Film Grade Applications: Blown film extrusion of T-shirt sacks, merchandise bags.Film properties below are based on a thickness of .8 mil and blow-up ratio of 4:1.Bapolene® and Bapolan® are registered tradem.. |
|||
Film Tensile Strength at Break, TD | >= 33.0 MPa | >= 4790 psi | |
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Film Tensile Strength at Break, TD | 33.0 MPa | 4790 psi | ASTM D882 |
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |