Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 90.0 g | 0.198 lb | F50; ASTM D 1709/A |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | 25µ; ISO 7765-1 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | 25µ; ISO 7765-1 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 90.0 - 100 g | 0.198 - 0.221 lb | ASTM D1709 |
Huntsman PE 1008 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
LyondellBasell Montell 16502F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709A |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ASTM D1709 A |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem F 7018 LDPE Extrusion Coating Polyethylene LDPE F 7018 is a low-density polyethylene and has excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating; and injec.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem F7018 LDPE Injection Molding Polyethylene F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem FG31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FG31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blow film extrusion in blends with polyethylene. It has excellent mechanical propert.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FM31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blown film extrusion. It has excellent mechanical properties, especially hot tack. I.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM-D1709 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D-1709A |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |
|||
Dart Drop Test | 90.0 - 126 g | 0.198 - 0.278 lb | Average value: 106 g Grade Count:6 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Dart Drop Test | 90.0 - 909 g | 0.198 - 2.00 lb | Average value: 336 g Grade Count:24 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | ASTM D1709 |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Dart Drop Test | 90.0 g | 0.198 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film