Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 300 g | 0.662 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Dart Drop Test | 300 g | 0.662 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring .. |
|||
Dart Drop Test | 300 g | 0.662 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical |
|||
Dart Drop Test | 300 g | 0.662 lb | ISO 7765-1 |
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709A |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709A |
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Dart Drop Test | 300 g | 0.662 lb | 1.0 mil; ASTM D 1709 |
Total L425 HDPE Film Blown film polyethylene grade. Provides excellent bubble stability, exceptional tear strength, high impact and puncture resistance, outstanding clarity and gloss, good stiffness, excellent compatibi.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
Formosa Plastics Formolene® E924ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
ExxonMobil Exceed™ 1023CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1023CA is a metallocene ethylene-hexene copolymers. The slightly higher stiffness of Exceed 1023CA makes it easier to process on certain filling machinery, whilst still k.. |
|||
Dart Drop Test | <= 300 g | <= 0.662 lb | ASTM D1709A |
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Dart Drop Test | 300 g | 0.662 lb | |
Dow Elite® 5200 Linear Low Density Polyethylene 5200 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. This resin offers high impact strength and good puncture resistance at moderate stretch levels for .. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709A |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin.. |
|||
Dart Drop Test | 300 g | 0.662 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have.. |
|||
Dart Drop Test | 300 g | 0.662 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-713 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App.. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
M. Holland Company LL217AA LLDPE
(discontinued **) Features: High Clarity, Copolymer, Good ProcessabilityUses: Film, Cast FilmApprovals: FDA 21 CFR 177.1521Processing Method: Blown Film and Cast FilmInformation provided by M. Holland. |
|||
Dart Drop Test | 300 g | 0.662 lb | ASTM D1709 |
M. Holland Company MAGMA® LM124-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |