Material Notes:
Features: High Clarity, Copolymer, Good ProcessabilityUses: Film, Cast FilmApprovals: FDA 21 CFR 177.1521Processing Method: Blown Film and Cast FilmInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 2.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.103 GPa
14.9 ksi
ASTM D882
Secant Modulus, TD 0.110 GPa
16.0 ksi
ASTM D882
Dart Drop Test 300 g
0.662 lb
ASTM D1709
Optical Properties Metric English Comments
Haze 1.8 %
1.8 %
ASTM D1003
Descriptive Properties Value Comments
Form Pellets