Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ASTM D1922 |
Reliance Industries Reclair F18010 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Applications:lamination films. Information provided by Reliance Industries |
|||
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-Y821-D Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good blocking resistance.Applications: Bags-on-roll, produce bags, garment film, trash bags.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ASTM D1922 |
Reliance Industries Reclair F19010 Polyethylene Blow film Linear Low Density Polyethylene grade. Reclair F19010 is butene comonomer based, with optimum levels of antioxidants, antiblocking agents, slip additives, and polymer processing aids. Th.. |
|||
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ISO 6383-2 |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ASTM 1922 |
Braskem LF 0720/20 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Elmendorf Tear Strength, MD | 3.30 g/micron | 83.8 g/mil | ASTM 1922 |
Braskem LF 0720/21 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); high clarity films; "liners"; general purpose. Information provided by Braskem |