Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 376 Polyester Film Melinex® 376 is a translucent, smooth, matte polyester film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 142 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 200 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 48 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 500 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 75 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa @Strain >=5.00 % |
15000 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 92 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge Melinex® FRP is designed specifically for embossing and release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling properties.Informati.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |