Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 19MB440 OPP Film Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 21MB621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec, PVdC; ExxonMobl Method |
ExxonMobil Bicor™ 21MB777 OPP Film Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
510 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 26MB600 OPP Film Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
PVdC, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 26MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
510 g/in @Pressure 40.0 psi, Temperature 266 °F |
Acrylic, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 26MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
510 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Seal Strength | 510 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
510 g/in @Pressure 40.0 psi, Temperature 284 °F |
PVdC, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 32MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin.. |