Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.20 GPa | 754 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Tensile Modulus | 5.20 - 18.2 GPa | 754 - 2640 ksi | MD |
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | |
Radici Radiflam® A RV250AF (cond.) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Tensile Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | |
LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled Dissipative product based on Polypropylene homopolymer (PPh). Mica filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 Type 1A |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Tensile Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ASTM-D790 |
Polyram RamOfin PPC364I6 Polypropylene, 30% Mineral and Glass Fiber 30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled Information provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWUVCP 25% Mineral and 15% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AK8 PA66, 40% Mineral Reinforced, Injection Molding Staramide AK8 is a 40% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GS 40 HWCP 40% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |