Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.14 GPa | 600 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NL-10GF/000 BLACK Polyamide 612 (Nylon 612) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | TM R050-36 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | TM R050-36 |
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem.. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E8 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D-638 |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
PolyOne Edgetek® UR-30GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 30% Glass Fiber Reinforced
(di Information provided by PolyOne™ Corporation |