Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® UR-30GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 30% Glass Fiber Reinforced  (di

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® UR-30GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 30% Glass Fiber Reinforced  (di.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne™ Corporation
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Tensile Modulus 4.14 GPa
600 ksi
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D648