Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.24 GPa | 470 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | Molded; ASTM D882 |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | |
Ineos ABS Lustran® SAN 51 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66 (Asia Pacific) LNP* Lubricomp* RAL22I is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated, High Impact. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP (Asia Pacific) LNP* THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Videolar 585 Crystal Polystyrene (GPPS) High heat extrusion crystalSuperior oriented polystyrene sheetFeatures: Low melt flowHigh molecular weightApplications: Foam applications such as egg cartons, meat trays and food serviceSuperior ori.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | |
Hexcel® HexPly® F155 Epoxy Resin HexPly® F155 is an advanced modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness and adhesive properties. HexPly.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Chevron Phillips EA3400 Medium Flow Crystal DescriptionChevron EA3400 is a medium flow-crystal polystyrene resin developed to blend with Styrene-Butadiene block copolymers for sheet extrusion and vacuum thermoforming. EA3400 can be used in c.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Ensinger TECAPET™ PET Polyethylene Terephthalate (PET) TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus,.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
Tensile Modulus | 3.24 GPa | 470 ksi | ASTM D638 |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |