Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex NSL121 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NSL121 is a compound based on PC+ABS Blend resin containing Stainless Steel Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Internall.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 9090 PEI Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM-D790 |
Polyram RamSter RF350M3 PBT, 15% Mineral Filled 15% mineral filled PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO R527 |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F).. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
Unitika A1030JR PA6, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM D638 |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM D638 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527 |
Radici Heraform® R 3000 Acetal Copolymer Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527 |
Polyram RamTough PZ304G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | |
LATI Latilub 73/13 Y/20 POM, 20% Aramid Fiber Reinforced Self-lubricating product based on Polyoxymethylene (POM). Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |