Mechanical Properties Metric English Comments
Tensile Modulus 2.87 GPa
416 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87707 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.87 GPa
416 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87717 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.87 GPa
416 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87727 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.87 GPa
416 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne
Tensile Modulus 2.87 GPa
416 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS
Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal ..
Tensile Modulus 2.87 GPa
416 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY FXW749SK ASA
Sparkle VisualFx ASA Resin - Weatherable
Tensile Modulus 2.87 GPa
416 ksi
ASTM Data
Americas Styrenics Styron® 615APR Polystyrene  (discontinued **)
STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of ..
Tensile Modulus 2.87 GPa
416 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT
LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant.
Tensile Modulus 2.87 GPa
416 ksi
ASTM D638
Teknor Apex APEX® RE 9016A Polyvinyl Chloride, Rigid
Features: Good Weather Resistance; High Impact Resistance Forms: PelletsInformation Provided by Teknor Apex
Tensile Modulus 2.87 GPa
416 ksi
1 mm/min
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo..
Tensile Modulus 2.87 GPa
416 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS
LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific.
Copyright © lookpolymers.com All Rights Reserved