Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 25.0 GPa | 3630 ksi | ISO 527-2 |
PolyOne OnForce™ LFT AM-30LCF/001 Grey Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | ISO 527 |
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | ASTM D638 |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | ISO 527 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Tensile Modulus | 25.0 GPa @Temperature 23.0 °C |
3630 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East) LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 25.0 GPa @Temperature 100 °C |
3630 ksi @Temperature 212 °F |
90º, Wet; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | ISO 527 |
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | longitudinal; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | longitudinal; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | longitudinal; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Tensile Modulus | 25.0 GPa | 3630 ksi | EN2597B |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581 Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel |