Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 124R PC UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HF1130R PC PC, High Flow, Mold Release, UV-Stabilized |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Tensile Modulus | 2.37 GPa @Thickness 3.20 mm |
344 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Tensile Modulus | 2.37 GPa | 344 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber. |