Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Tensile Modulus | 1.31 GPa @Temperature 23.0 °C |
190 ksi @Temperature 73.4 °F |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | 1% Secant; 0.5"/min; ASTM D638 |
LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 µm) .. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | 2 in/min; ASTM Test |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Dow TF0807 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I.. |
|||
Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |