Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.8 GPa | 1710 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Tensile Modulus | 11.79 GPa | 1710 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Tensile Modulus | 11.79 GPa | 1710 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | ISO 527-1/-2 |
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | ASTM D638 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN LT51G35HSLR BL661A Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Laser Weldable PPA High Performance Polyamide Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | ISO 527-1 |
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced PEEK-GF30Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 11.8 GPa @Temperature 23.0 °C |
1710 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | ASTM D638 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | ISO 527-1/2 |
Radici Radiflam® BRV300 AE Polybutylene Terephthalate PBT Self-extinguishing glass-fiber reinforced with halogenInformation provided by Radici group. |
|||
Tensile Modulus | 11.8 GPa | 1710 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East) LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |