Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.90 GPa | 1000 ksi | |
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ H PC DP105/X3 BK Polycarbonate Polycarbonate-Black colored, thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Tensile Modulus | 6.92 GPa @Thickness 6.40 mm |
1000 ksi @Thickness 0.252 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL933 PC Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | ASTM D638 |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | ASTM D638 |
Ensinger Tecatron® XP-66 Compression Molded PPS Compound, 30% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 6.90 GPa @Temperature -40.0 °C |
1000 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned) Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Tensile Modulus | 6.90 GPa | 1000 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-10CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation. |