Ensinger Tecatron® XP-66 Compression Molded PPS Compound, 30% Fiberglass

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-66 Compression Molded PPS Compound, 30% Fiberglass.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength 36.5 MPa
5300 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Tensile Modulus 6.89 GPa
1000 ksi
ASTM D638
Flexural Strength 64.8 MPa
9400 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Descriptive Properties Value Comments
Color Dark Brown