Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.30 GPa | 1350 ksi | |
Plastcom SLOVAMID 6 GF 30 FRA 5 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
Nilit FRIANYL B63 HS-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP (Asia Pacific) LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ASTM D638 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | dry; ISO 527-1/-2 |
DSM Akulon® N24-G6 PA6-GF30 30% Glass Reinforced |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ASTM D638 |
BLUESTAR 201-G20202 PBT, 20% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |