Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.20 GPa | 464 ksi | |
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-2 |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-2 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-2 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
Grupo Repol Dinalon® C1S25 PA6/PA66 Blend, Unreinforced Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | |
LATI Latigray 75/4-01 CX/45 PBT Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 221 Natural FA PA66, DRY Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 9011 PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
Styrolution PS 153A GPPS Styrolution PS 153A is an antistatic modified, general purpose polystyrene grade with a good flow characteristic.AntistaticGood flow characteristicsInformation provided by Styrolution |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
Solvay Technyl® A 205F Nylon 66, EH0 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527-1, 2 |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ASTM-D790 |
Polyram PlusTek PB847I4 Nylon 6, 20% Glass Fiber and Mineral 20% glass fiber and mineral reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1013C5 PA6 Injection Molding, Easy Molding Grade |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ HMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness, high heat stabilization, low emissions and low odor for automotive HVAC and under-the-hood applic.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ASTM Test |
BASF Ultramid® A27 E 01 PA66 (Dry) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527 |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |