Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 21.84 GPa | 3168 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S.. |
|||
Tensile Modulus | 21.84 GPa | 3168 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 21.84 GPa | 3168 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
Tensile Modulus | 21.84 GPa | 3168 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |