Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.5 GPa | 2250 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | |
LATI Latilub 66-01M G/50 PA66, 50% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber Description: Partly aromatic Polyamide 6.6 Copolymer, 41% glass fiber reinforced and flame retardants.Application:Stiff molding parts with high stiffness by outstanding thermal stability, reduced w.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4105 black 9992 PA610-GF50 Product description: Grilamid XE 4105 black 9992 is a 50% glass fiber reinforced, heat stabilized and UV resistant polyamide 610 (PA610) injection molding grade. This product is to a large extent ba.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 545 BK504 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness excellent dimensional stability and cr.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 15.5 GPa | 2250 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and.. |
|||
Tensile Modulus | 15.5 GPa @Temperature 23.0 °C |
2250 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |