Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.5 GPa | 2100 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | tangent; ASTM D638 |
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | tangent; ASTM D638 |
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1,-2 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Tensile Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI (Asia Pacific) LNP* Thermocomp* EC004XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40 Product description: Grivory HTV-4H1 black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40 Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |