Polymer Property : Tensile Modulus = 13.78 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC
LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific)
LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX05474 PC
LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold ..
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific)
LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret..
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Modulus 13.78 GPa
1999 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK
LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA
LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific)
LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV008ES PA 66
LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 (Asia Pacific)
LNP* THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.