Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.130 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5117N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4117P (18402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118P (18402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus 0.130 GPa

@Temperature 120 °C
18.9 ksi

@Temperature 248 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Modulus 0.130 GPa
18.9 ksi
1 mm/min
Arkema Group Evatane® 1020 VB 3 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding rigid articles. Examples: closures, ice trays.ISO data provided by the manufacturer, Arkema.
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Copyright © lookpolymers.com All Rights Reserved