Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.14 - 57.0 MPa | 600 - 8270 psi | Average value: 19.9 MPa Grade Count:13 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
7690 - 8270 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa @Thickness 2.00 mm |
7690 - 8270 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition.. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa @Thickness 2.00 mm |
7690 - 8270 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Tensile Strength, Yield | 55.0 - 57.0 MPa | 7980 - 8270 psi | ASTM D638 |
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 500 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
7690 - 8270 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa | 7690 - 8270 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa | 7690 - 8270 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa | 7690 - 8270 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa | 7690 - 8270 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |