Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.9 MPa | 8400 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM Data |
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Tensile Strength, Yield | 57.9 MPa @Thickness 3.17 mm, Temperature 22.8 °C |
8400 psi @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D638 |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Techmer ES HiFill® PA6 0301 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Techmer ES Luriblend® POM CO TL15 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 1000 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 1950 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM Data |
Styron CALIBRE™ IM 401 18 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength an.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Resin Overview: CALIBREâ„¢ IM 401-18 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Tensile Strength, Yield | 57.9 MPa @Temperature 23.0 °C |
8400 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3501 GF-10 Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |
|||
Tensile Strength, Yield | 57.9 MPa @Temperature 149 °C |
8400 psi @Temperature 300 °F |
ASTM D638 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 57.9 MPa | 8400 psi | ASTM D638 |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |