Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.2 - 72.4 MPa | 8010 - 10500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC) Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne |
|||
Tensile Strength, Yield | 55.2 MPa @Thickness 3.17 mm |
8010 psi @Thickness 0.125 in |
ASTM D638 |
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.2 MPa @Thickness 3.17 mm |
8010 psi @Thickness 0.125 in |
ASTM D638 |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | ASTM D638 |
PTS Trilac® TR558-CL ABS- Transparent ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.2 MPa @Thickness 3.17 mm |
8010 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ 83510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 55.2 MPa @Temperature 23.0 °C |
8010 psi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC MC500 Polyvinyl Chloride, Chlorinated (CPVC) The Geon MC500 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon MC500 demonstrates superior processa.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ LC-5000C TC LCP
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Strength, Yield | 55.2 MPa @Thickness 3.20 mm |
8010 psi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | ASTM D638 |
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | ASTM D-638 |
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4526 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high res.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |