Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Niagara LaSalle 1213 Cold Finished Steel Bar The A.I.S.I. grade 1215 has essentially eliminated a number of similar free machining grades, such as 1212. Both 1215 and 1213 machine considerably faster than 1212 and provide good surface finish a.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Pacific Sintered Materials FCC-214-S High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Pacific Sintered Materials FX-232-T Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-50All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 414 MPa @Temperature 23.9 °C |
60000 psi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
Materion BrushBronze® 630 (AMS 4640) 1.0" - 2.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Yield | 414 - 483 MPa @Strain 0.200 % |
60000 - 70000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 414 - 483 MPa @Strain 0.200 % |
60000 - 70000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 414 - 517 MPa | 60000 - 75000 psi | |
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 %, Temperature 538 °C |
60000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | |
HP Alloys Alloy 718, 0% Cold Worked, Not Aged 0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes .. |
|||
Tensile Strength, Yield | 414 - 896 MPa @Strain 0.200 % |
60000 - 130000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Tensile Strength, Yield | >= 414 MPa | >= 60000 psi | |
ThyssenKrupp 12Ni5 Structural Steel 5% nickel steel for low temperature service down to -165°FApplication for pressure vessels and tanks for the transportation and storage of ethyleneReference: 5.000 t/y in thicknesses up to 2 in.Hea.. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | AR-5% O2 |
Universal Wire Works ER90SB-9 Steel Welding Wire Universal 90S-B9 is used primarily for welding the higher chromium alloyed 9CrMoNbV steels A213 (T-91), A335 (p-91), A387 (Gr-91) used where elevated temperatures and pressures are required. The adv.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Universal Wire Works Inconel 718 (AMS 5832) Filler Metal Inconel Filler Metal 718 is recommended for gas tungsten arc and gas metal arc welding of alloy 718, 706 and X-750. This double gamma prime alloy has excellent strength, good ductility up to 1300°F.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Universal Wire Works 347 Stainless Steel (AMS 5680) Filler Metal Universal 347 is extensively used with the gas tungsten arc, gas metal arc and submerged arc processes. This alloy is suitable for welding stabilized steel grades 321, 347 and 348. Alloy 347 should .. |
|||
Tensile Strength, Yield | >= 414 MPa | >= 60000 psi | 0.2% offset |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Yield | 414 - 469 MPa | 60000 - 68000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, Extra Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 414 - 462 MPa | 60000 - 67000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 414 - 607 MPa | 60000 - 88000 psi | 0.2% offset |
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick) |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal Data provided by Allvac.Applications: High temperature applications, jet engine components, devices in high fatigue service. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Yield | >= 414 MPa | >= 60000 psi | For flat products (<4" thickness) and seamless tube and pipe |
ATI Allegheny Ludlum AL Altemp® 625 Nickel-Base Superalloy, UNS N06625 Allegheny Ludlum Altemp 625 alloy is an austenitic nickel-base superalloy possessing excellent resistance to oxidation and corrosion over a broad range of corrosive conditions, including jet engine .. |
|||
Tensile Strength, Yield | 414 MPa | 60000 psi | Solution Annealed |
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy Characteristics: high strength up to 1500°F, oxidation resistance up to 2000°FInformation provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 %, Temperature 260 °C |
60000 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe.. |