Material Notes:
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typical uses are for architectural ornamental trim, emblems, plaques, connectors, rotor bars, AC motors, fasteners, bullet jackets, fuse caps, firing pins, and coins.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 65 - 69
65 - 69
Thickness > 0.020 Inch
Tensile Strength, Ultimate 421 - 476 MPa
61000 - 69000 psi
Tensile Strength, Yield 414 - 469 MPa
60000 - 68000 psi
0.2% offset
Elongation at Break >= 2.0 %
>= 2.0 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 233 W/m-K
1620 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 95 %
95 %
Zinc, Zn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000318 ohm-cm
0.00000318 ohm-cm