Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 48000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 331 MPa

@Temperature 23.9 °C
48000 psi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 7781 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Tensile Strength, Yield 331 MPa

@Strain 0.200 %,
Temperature 538 °C
48000 psi

@Strain 0.200 %,
Temperature 1000 °F
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched
Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Tensile Strength, Yield 331 MPa

@Strain 0.200 %,
Temperature 538 °C
48000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 331 MPa

@Strain 0.200 %,
Temperature 538 °C
48000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 331 MPa

@Strain 0.200 %,
Temperature 316 °C
48000 psi

@Strain 0.200 %,
Temperature 601 °F
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 331 MPa

@Strain 0.200 %
48000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 331 MPa

@Strain 0.200 %
48000 psi

@Strain 0.200 %
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926)
Data provided by the manufacturer, Special Metals.
Tensile Strength, Yield >= 331 MPa
>= 48000 psi
Wingate Alloys Winco NT 24 Nitrogen-Strengthened Austenitic Stainless Steel
Winco NT 24 provides good aqueous corrosion resistance combined with resistance to abrasives, metal-to-metal wear and sustained heats of 1500°F. Higher mechanical properties than standard austeniti..
Tensile Strength, Yield >= 331 MPa
>= 48000 psi
Alcoa Deltalloy® 4032-T651 Aluminum
Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist..
Tensile Strength, Yield 331 - 393 MPa
48000 - 57000 psi
0.2% offset
Eagle Brass 110 EPT COPPER, Spring
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Tensile Strength, Yield 331 - 400 MPa
48000 - 58000 psi
0.2% offset
Eagle Brass 240 Low Brass, 3/4 Hard
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Tensile Strength, Yield 331 - 538 MPa
48000 - 78000 psi
0.2% offset
Eagle Brass 752 Nickel Silver 18%, 1/2 Hard
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Tensile Strength, Yield 331 - 393 MPa
48000 - 57000 psi
0.2% offset
Eagle Brass 101 OFE COPPER (Certified), Spring
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Yield 331 - 393 MPa
48000 - 57000 psi
0.2% offset
Eagle Brass 102 OF COPPER (Non-Certified), Spring
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Tensile Strength, Yield 331 MPa

@Strain 0.200 %
48000 psi

@Strain 0.200 %
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched
Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re..
Tensile Strength, Yield 331 MPa
48000 psi
In rolling direction
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Tensile Strength, Yield 331 MPa
48000 psi
In rolling direction
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Tensile Strength, Yield 331 MPa
48000 psi
In rolling direction
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Tensile Strength, Yield 331 MPa
48000 psi
Semi-Processed
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel
Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard grades from M-15 to M-47 ..
Tensile Strength, Yield 331 MPa
48000 psi
Typical
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel
Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab..
Tensile Strength, Yield >= 331 MPa

@Strain 0.200 %
>= 48000 psi

@Strain 0.200 %
Carlson Nitronic® 30® Austenitic Stainless Steel
General DescriptionNitronic 30 is a nitrogen-strengthened austenitic stainless steel developed for applications requiring good aqueous corrosion resistance combined with good resistance to abrasive ..
Tensile Strength, Yield 331 MPa
48000 psi
In rolling direction
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Copyright © lookpolymers.com All Rights Reserved