Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 235 MPa | >= 34100 psi | |
MetalTek MTEK 35-15 Cast UNS N08605 Heat Resistant Stainless Steel Good strength at heat treating temperatures. Resists thermal shock of repeated heating and cooling.Applications: Dampers, pots, blades, rolls, door frames, retorts, rolling mill guides.Information p.. |
|||
Tensile Strength, Yield | >= 235 MPa | >= 34100 psi | |
MetalTek MTEK 35-50W Heat Resistant Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 235 MPa @Strain 0.200 %, Temperature 870 °C |
34100 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 235 MPa @Temperature 870 °C |
34100 psi @Temperature 1600 °F |
|
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 188/ Multimet alloy 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 235 MPa @Strain 0.200 %, Temperature 760 °C |
34100 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Tensile Strength, Yield | >= 235 MPa | >= 34100 psi | |
MetalTek MTEK 25-35 Cast UNS N08705; Cast UNS J95705 Heat Resistant Stainless Steel Higher chrome and nickel content provides increased strength and resistance to both oxidation and carburization.Applications: Reformer and Ethylene pyrolysis tubes and fittings.Information provided .. |
|||
Tensile Strength, Yield | >= 235 MPa | >= 34100 psi | |
MetalTek MTEK 35-45MA Heat Resistant Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | ISO 527-2 |
Solvay Specialty Polymers Omnix® 9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® 9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture ab.. |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | ISO 527-2 |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF55 L BK 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® MKD-1015 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® MKD-1015 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | ASTM D638 |
Cheng Yu Plastic NG1500S Nylon 66, 50% Glass Fiber Reinforced |
|||
Tensile Strength, Yield | 235 MPa | 34100 psi | Dry; ASTM D638 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |