Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.0 MPa | 3050 psi | 50 mm/min; ISO 527 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D412 |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
LyondellBasell SEQUEL® E3000 FR TPO Description: SEQUEL® E3000FR thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spe.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global) Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-9523 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9523 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9523 is dev.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
Flint Hills P6E2A-005 Impact Copolymer Polypropylene Impact copolymer, UL certified.Features: LTHA and extra high impact strength.Applications: Injection molding and extrusion: high pressure resistance, film, and flexible profiles.Former Huntsman poly.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ SP98F/94 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ SP98F/94 Black medium melt flow, 2,300 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of stiffness, impact .. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | 50mm/min; ISO 527-2 |
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This .. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ISO 527 |
Unipetrol PP MONSTEN® GB 608 Polypropylene Impact Copolymer Made for injection molding applications. Slip and antiblocking agent stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP25-0715CF20 20% Conductive Filler Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
Dow C719-35RNHP Polypropylene High Impact Contains nucleating agent Controlled rheology product Complies with U.S. FDA 21 CFR 177.1520 © 3.1a Information provided by DowDow Announced Sale of Global Polypropylene Business to B.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | |
Dow DOWLEX™ IP-10262 High Density Polyethylene DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | |
Dow DOWLEX™ IP-90 High Density Polyethylene Next Generation DOWLEX® IP-90 resin is a high flow improved processing high density polyethylene resin designed for ultra-thin wall injection molded containers and drink cups. This resin has been m.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D638 |
Clariant Remafin PP1100NAT Polypropylene Impact Modified Copolymer Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ISO R 527 |
Arkema Group OREVAC® 18750 Maleic Anhydride Modified Polypropylene DescriptionOREVAC 18750 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resi.. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ISO R 527 |
Addiplast Addilene H 520 T40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | |
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 21.0 MPa | 3050 psi | ASTM D-638 |
Axiall 35551 Wire & Cable Flexible PVC TW, THW insulation compound suitable for 105°C AWM applications. Oil II rated and VW-1. CSA approved for TR64, TR32, TEW, and AW.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |