Material Notes:
Next Generation DOWLEX® IP-90 resin is a high flow improved processing high density polyethylene resin designed for ultra-thin wall injection molded containers and drink cups. This resin has been molded into containers exceeding flow length/container wall thickness ratios of 350, while demonstrating good impact and load properties. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.1(a) for food contact applications. The regulation should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Melt Flow 90 g/10 min

@Load 2.16 kg
90 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.0 MPa
1450 psi
Tensile Strength, Yield 21.0 MPa
3050 psi
Elongation at Break 150 %
150 %
Modulus of Elasticity 0.621 GPa
90.1 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.910 GPa
132 ksi
Izod Impact Resistance 1.10 J/cm²
5.24 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F