Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx60FRDUV Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W1820L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WY66AL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable Y66A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WY66L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D638 |
Resirene Resirene® READ 9500 Ignition Resistant Impact Polystyrene Features:High FlowIgnition ResistantNo Pre-drying RequiredHigh ImpactColors AvailableApplications:Injection MoldingDark ColorsTV CabinetsElectronic EquipmentInformation provided by US distributor Ca.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R7400B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D638 |
LyondellBasell Purell® PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 3020 D is a low density polyethylene with high rigidity, good opticals and good chemical resistance. It is delivered in pellet form. Target markets are small blow molding including packagi.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D 638 |
LyondellBasell Adflexâ„¢ KS311P Polyolefin Description: Adflexâ„¢ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell proces.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Mul.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D412 |
Teknor Apex APEX® 3310-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3311-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D412 |
Teknor Apex Flexalloy® 3500-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | Longitudinal |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.004" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D638 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D638 |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D-638 |
Axiall 16860 Wire & Cable Flexible PVC Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D-638 |
Axiall 801-90B Moldings & Extrusions Flexible PVC Automotive harness tape.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D-638 |
Axiall 8800 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D-638 |
Axiall 8900 Moldings & Extrusions Flexible PVC General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Tensile Strength, Yield | 15.2 MPa | 2200 psi | ASTM D-638 |
Axiall 491 Wire & Cable Flexible PVC 60°C rated low temperature jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |