| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible R7400B Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 67 | 67 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 400 % | 400 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
| Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
| Oxygen Index | 24 % @Thickness 1.91 mm |
24 % @Thickness 0.0752 in |
ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 6.40e+11 ohm-cm | 6.40e+11 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 155 - 165 °C | 311 - 329 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | UL QMTT2 | |
| Change in Flexural Strength | 100% | ASTM D543; 60°C, 1.91 mm; in ASTM Oil #2, 168 hr |
| Change in Ultimate Elongation | -19% | ASTM D543; 60°C, 168 hr, in ASTM #2 Oil; 0.075 in |
| Features | Flame Retardant | |
| Sunlight Resistant (720 hours) | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 89% | 121°C, 1.91 mm; 500 hr, UL Standard |
| Retention of Tensile Strength | 110% | 121°C, 1.91 mm; 500 hr, UL Standard |
| Uses | Cable Jacketing | |
| Flexible Cord Jacketing | ||
| Wire & Cable Applications | ||
| Wire Types | SJT | |
| SJTO |