Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.3 MPa
1490 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W7400 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 10.3 MPa
1490 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-UR-080-W Polyurethane, Unspecified (PUR, Unspecified)
Information provided by PolyOne
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D412
Polymax® Maxelast® F02-129E-1C TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D412
Precision Polymer Engineering H70B Epichlorohydrin
Peroxide Cured, Epichlorohydrin Rubber, 65-75 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. ASTM and ISO designation = GECO.Applications: Excellent resistance t..
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D638
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin
Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film..
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D638
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin
Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer.
Tensile Strength, Yield 10.3 MPa
1490 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman 1870A Polyethylene  (discontinued **)
Polyethylene 1870A is a low density formulation with excellent flow characteristics for injection molding. It is used for such applications as container closures that require stress-crack resistanc..
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D638
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin  (discontinued **)
NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat..
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D638
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade
Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific..
Tensile Strength, Yield 10.3 - 22.5 MPa
1490 - 3260 psi
ISO/R 527E
Mikro-Technik Reproflon PTFE
Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D412
Teknor Apex APEX® 94-A0098C-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding..
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D412
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D412
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 10.3 MPa
1490 psi
2.0 in/min; ASTM D638
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tensile Strength, Yield 10.3 MPa
1490 psi
2.0 in/min; ASTM D638
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tensile Strength, Yield 10.3 MPa
1490 psi
Zylog Hipolyene® 2703 MS EX 3 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 10.3 MPa
1490 psi
Zylog Hipolyene® 2703 MS Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 10.3 MPa
1490 psi
Molded property
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. ..
Tensile Strength, Yield 10.3 MPa
1490 psi
Molded property
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1..
Tensile Strength, Yield 10.3 MPa
1490 psi
Dow LDPE 779I Low Density Polyethylene
DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps..
Tensile Strength, Yield 10.3 MPa
1490 psi
2 in/min (50 mm/min); ASTM D638
Bapolene® 1052 Polyethylene, Injection Grade
A medium flow general purpose injection molding resin with good gloss, toughness and good chemical resistance. This product meets FDA standards for food contact applications.Applications: Caps and ..