Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.0 - 20.0 MPa | 1450 - 2900 psi | 50 mm/min; ISO/R 527 |
Okulen® 500 - REG PE Multicoloured fine OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Tensile Strength, Yield | >= 10.0 MPa | >= 1450 psi | ASTM D412 |
Precision Polymer Engineering C70H Chloroprene Rubber Off-white, Chloroprene Rubber, 65-75 °IRHD. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regu.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering E80K Ethylene Propylene Rubber General purpose, peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet ASTM D2000/SAE J200 line call-out MCA810, A25, B35, F17... |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering N80L Nitrile Rubber Nitrile Butadiene Rubber, 75-85 °IRHD. Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000 line call-out M6BG814, A14, B14, EO14, EO34, F17.Applications: T.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering S65T Silicone Rubber Translucent Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United Sta.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V60E Fluoroelastomer Compound Litharge Incorporated, Green Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B38, EF31, EO78, F15, Z.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V60F Fluoroelastomer Compound Peroxide/Litharge cured, Fluoroelastomer Rubber, 55-65 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V60G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 56-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B38, EF31, EO78, F15, Z1. Where Z1 = colour gr.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V75M Fluoroelastomer Compound Brown Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z1, Z2. Z1 = comp.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | 500 mm/min; ASTM D638 |
Eastman D4027-P Voridian Polyethylene
(discontinued **) VORIDIAN low density polyethylene D4027-P is a formulation suggested for extrusion coating applications that require clarity, high gloss and superior hot tack properties. Applications/UsesFood Packa.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 808A Polyethylene
(discontinued **) Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE 1008 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE 1011 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE1058 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE2018 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliantFeatures: Good toughness and machinabilityApplications: Injection molding: closures and small items.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under co.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Braskem BI 818 LDPE Injection Molding Polyethylene
(discontinued **) Applications: Injection molding; masterbatches. Information provided by Braskem |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Kraton® D1102 + LDPE blend (4/96) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® A 5703 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 6019 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg B545 High Quality Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg E935 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg Hypalon® H730 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg R449 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg B870 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | 50 mm/min |
Arkema Group Evatane® 1005 VL 2C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for thermal agricultural films to 180 at 200 µ with diffusing effect, for greenhouse coverage.ISO d.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Teknor Apex APEX® 3210-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 10.0 - 23.0 MPa | 1450 - 3340 psi | Average value: 13.3 MPa Grade Count:9 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Global J-4324 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Tensile Strength, Yield | 10.0 - 85.3 MPa | 1450 - 12400 psi | Average value: 26.8 MPa Grade Count:173 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |