Material Notes:
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON D series consists of an unsaturated polymer, either butadiene or isoprene, as the rubber monomer. Unless otherwise specified, All properties listed below are measured on blown film, 4 mil (100 microns) thick. Information provided by the manufacturer, Kraton® Polymers.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.0 MPa
1450 psi
Tensile Impact Strength 128 kJ/m²
60.9 ft-lb/in²
Dart Drop Test 275 g
0.606 lb
Using 2 in. (0.508 cm) dia dart, 60 in. (774 cm) drop height.