Material Notes:
EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and low temperature ranges.Special compounding can increase some grades to function continually at +140°CE.P's are inherently resistant to attack by oxygen, U.V., Ozone and extreme weather environments, and will give long service in these conditions.E.P's do not have good adhesion properties and expert advice should be sought from Trelleborg's Technical Department about bounding applications.Resistance to Chemicals; resistant to many chemicals and solvents. Good resistance to many corrosive chemicals. The performance of E.P's in hot water and high pressure steam is better than in dry heat.All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Tensile Strength, Yield 10.0 MPa
1450 psi
Elongation at Break 200 %
200 %
Tear Strength 30.0 kN/m
171 pli
Compression Set 48 %

@Temperature 70.0 °C,
Time 79200 sec
48 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Descriptive Properties Value Comments
Color Black