Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 790 - 940 MPa | 115000 - 136000 psi | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 77%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | >= 790 MPa | >= 115000 psi | |
MetalTek MTEK CA20NW Cast UNS J91631 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | 795 MPa | 115000 psi | |
Haynes Hastelloy® W alloy, gas tungsten arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 795 MPa @Strain 0.200 %, Temperature 760 °C |
115000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 793 MPa @Temperature 899 °C |
115000 psi @Temperature 1650 °F |
oil quench, tempered at 1200°F |
Latrobe Nitralloy® N™ VAC-ARC Premium Nitriding Steel NITRALLOY N is an age hardenable nitriding steel. The age hardening capability of the alloy permits the core strength to be developed while the surface is being nitrided. VAC-ARC remelting is employ.. |
|||
Tensile Strength, Yield | 790 - 1040 MPa | 115000 - 151000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 790 - 1040 MPa | 115000 - 151000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 793 - 1172 MPa | 115000 - 170000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way).. |
|||
Tensile Strength, Yield | 790 MPa @Strain 0.200 %, Temperature 540 °C |
115000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 793 - 1030 MPa @Strain 0.200 % |
115000 - 150000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Tensile Strength, Yield | 790 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals MONEL® Alloy K-500 A precipitation-hardenable nickel-copper alloy that combines the corrosion resistance of MONEL alloy 400 with greater strength and hardness. It also has low permeability and is nonmagnetic to under.. |
|||
Tensile Strength, Yield | 793 - 931 MPa @Strain 0.200 %, Thickness >=25.4 mm |
115000 - 135000 psi @Strain 0.200 %, Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Tensile Strength, Yield | 793 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
Annealed |
Universal Wire Works 5Al-2.5Sn (AMS 4953) Titanium Alloy Filler Metal Universal Ti 5Al-2.5Sn titanium alloy is easily joined with the gas tungsten arc, gas metal arc or resistance welding processes. 100% joint efficiency can be obtained provided proper shielding proce.. |
|||
Tensile Strength, Yield | >= 795 MPa @Strain 0.200 % |
>= 115000 psi @Strain 0.200 % |
Longitudinal |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Tensile Strength, Yield | >= 793 MPa | >= 115000 psi | 0.2% offset |
Eagle Brass 770 Nickel Silver 18%, Extra Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Yield | 793 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 792 - 861 MPa @Strain 0.200 % |
115000 - 125000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS01 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 793 MPa | 115000 psi | 0.2% Offset |
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical. |
|||
Tensile Strength, Yield | 793 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
|
ATI Allvac® 6-7 UNS R56700 Titanium Alloy Uses: Biomedical implants. Femoral hip stems, fracture fixation plates, spinal components, fasteners, nails, rods, screws, wire.Property values are for samples in the metallurgical condition: 1300°.. |
|||
Tensile Strength, Yield | 793 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Turbine, engine components. Blades, vanes, fasteners, springs, bellows. Extrusion dies, nuclear, heat treating, forming tools. |
|||
Tensile Strength, Yield | 793 MPa @Strain 0.200 % |
115000 psi @Strain 0.200 % |
|
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age Data provided by Allvac.Applications: Jet and rocket engines, torque rings, afterburners, and hardware; space shuttle turbo pumps seals. |
|||
Tensile Strength, Yield | 792 - 930 MPa @Strain 0.200 % |
115000 - 135000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TM08 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 795 MPa | 115000 psi | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Tensile Strength, Yield | 793 MPa @Strain 0.200 %, Temperature 427 °C |
115000 psi @Strain 0.200 %, Temperature 801 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | >= 790 MPa | >= 115000 psi | |
MetalTek MTEK H46 Martensitic Stainless Steel "400" series, General corrosion resistant alloy, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTek.. |