Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 760 MPa | >= 110000 psi | |
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 755 MPa | 110000 psi | |
Haynes Hastelloy® W alloy, gas metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 760 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 758 - 965 MPa @Strain 0.200 % |
110000 - 140000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Tensile Strength, Yield | 758 MPa | 110000 psi | Cold Worked |
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd.. |
|||
Tensile Strength, Yield | 760 MPa @Strain 0.200 %, Temperature 650 °C |
110000 psi @Strain 0.200 %, Temperature 1200 °F |
Precipitation Hardened prior to test |
Special Metals INCONEL® Alloy 751 A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-.. |
|||
Tensile Strength, Yield | 758 - 896 MPa @Strain 0.200 % |
110000 - 130000 psi @Strain 0.200 % |
Heat Treatment (Condition T HRc 26-32) |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32) High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f.. |
|||
Tensile Strength, Yield | >= 759 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
Longitudinal |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A .. |
|||
Tensile Strength, Yield | >= 760 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
L and LT Directions |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Tensile Strength, Yield | >= 760 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
L, LT and ST Directions |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Tensile Strength, Yield | >= 759 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
L and LT Directions |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 302 Austenitic Stainless Steel, 1/2 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 304 Austenitic Stainless Steel, 1/2 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 316 Austenitic Stainless Steel, 1/2 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, 1/2 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | 760 - 830 MPa @Strain 0.200 % |
110000 - 120000 psi @Strain 0.200 % |
|
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 304L Austenitic Stainless Steel, 1/2 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Tensile Strength, Yield | 760 MPa | 110000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Tensile Strength, Yield | 760 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
Carpenter Pyromet® CTX-3 Superalloy, Heat Treatment for Brazing Cycles over 982°C Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
Tensile Strength, Yield | 760 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400 Property data below is typical of annealed samples. Available in plate. For use in fasteners, fittings, military equipment and air frame parts.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 759 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401) The ELI grade has lower impurity limits than standard titanium 6-4.Uses: applications requiring excellent fracture toughness and fatigue strength, aircraft, structural components, biomedical.Mechani.. |
|||
Tensile Strength, Yield | 759 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Jet engines, superchargers, missile components, fasteners, cryogenic equipment, nuclear, corrosive deep well hardware. |
|||
Tensile Strength, Yield | 759 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® W-722 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Ring components in jet engines. |
|||
Tensile Strength, Yield | 760 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 15-5 High Strength Stainless Steel, UNS S15500 Property data below is typical of annealed samples. Available in plate. For use in fasteners, military equipment and air frame parts.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 758 MPa | 110000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Yield | 760 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |
|||
Tensile Strength, Yield | >= 758 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT110 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |