Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.60 MPa | 1100 psi | ASTM D412 |
Precision Polymer Engineering N70U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade A1 (specification inactive for new design).Application.. |
|||
Tensile Strength, Yield | 7.60 MPa | 1100 psi | ASTM D412 |
Precision Polymer Engineering N85U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 75-95 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade B1 (specification inactive for new design).Applications.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D638 |
M. Holland Company LL508 LLDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 3.1bProcessing Method: Injection MoldingInformation provided b.. |
|||
Tensile Strength, Yield | 7.60 MPa | 1100 psi | ASTM D638-61T |
Chevron Phillips MarFlex® 1010 LDPE Extrusion Coating Resin
(discontinued **) Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Tensile Strength, Yield | 7.60 MPa | 1100 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 812P Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet... |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® E38 Perfluoroelastomer Chemraz® E38 was specifically developed for high-density plasma systems and diffusion processes where seal reliability and very minimal contamination are essential. The material provides excelle.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | Elastic; ASTM D638 |
Multibase Multi-Flex® A 5904 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone Resistant Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7206 E TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 8502 A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | >= 7.58 MPa | >= 1100 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7130 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex APEX® 3300-45 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex APEX® 3310-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | 100%; ASTM D412 |
Teknor Apex MF 569 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2770 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2780 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHM 7700 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex TEKBOND® MP 1726 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex TEKBOND® MP 1726 UVF Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | Type 1, 20 in/min; ASTM D638 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | Type 1, 20 in/min; ASTM D638 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Vidux® CV-1000-91 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 7.60 MPa | 1100 psi | ASTM D412 |
Vicone High Performance Rubber VicoSeal™ 003R-BK High Performance EPDM Rubber Two Material Product:Material 1: VicoSeal™ 003R-30 DUROMaterial 2: 11 ga CRS yellow anodized natural rubber vulcanized to yellow anodized steel (RoHS Approved)Information provided by Vicone |
|||
Tensile Strength, Yield | 7.60 MPa | 1100 psi | ASTM D638-61T |
Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D-638 |
Axiall 8540 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 7.60 - 12.0 MPa | 1100 - 1740 psi | Average value: 9.81 MPa Grade Count:21 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Tensile Strength, Yield | 7.58 MPa | 1100 psi | ASTM D-638 |
Axiall 83-126K Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 7.58 MPa @Strain 300 % |
1100 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-4080 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma.. |