Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505-60T
Moisture Vapor Transmission 0.550 cc-mm/m²-24hr-atm
1.40 cc-mil/100 in²-24hr-atm
at 14.2 lbs/ream coating (1.0 mil); ASTM E96-53T
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238-57T
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.30 MPa
1350 psi
ASTM D638-61T
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D638-61T
Elongation at Break 650 %
650 %
ASTM D638-61T
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ASTM D1525