Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 1100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D412
Precision Polymer Engineering N70U Nitrile Rubber
Nitrile Butadiene Rubber (NBR) 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade A1 (specification inactive for new design).Application..
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D412
Precision Polymer Engineering N85U Nitrile Rubber
Nitrile Butadiene Rubber (NBR) 75-95 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade B1 (specification inactive for new design).Applications..
Tensile Strength, Yield 7.60 MPa
1100 psi
M100
3M Dyneon™ Fluorel™ FC-2179 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested ..
Tensile Strength, Yield 7.58 MPa
1100 psi
at 100%; ASTM D412
EG93A Polyurethane-based Biomedical Elastomer
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D638-61T
Chevron Phillips MarFlex® 1010 LDPE Extrusion Coating Resin  (discontinued **)
Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che..
Tensile Strength, Yield 7.58 MPa
1100 psi
@ 50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 510 Perfluoroelastomer
Greene Tweed’s Chemraz® 510, a perfluoroelastomer, offers an extremely broad range of chemical resistance with a Shore A hardness value of 90. with a temperature range form -22°F to 446Â..
Tensile Strength, Yield 7.58 MPa
1100 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® E38 Perfluoroelastomer
Chemraz® E38 was specifically developed for high-density plasma systems and diffusion processes where seal reliability and very minimal contamination are essential. The material provides excelle..
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D 638
LyondellBasell Adflexâ„¢ Q 200 F Polyolefin
Description: Adflexâ„¢ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's propri..
Tensile Strength, Yield 7.58 MPa
1100 psi
Elastic; ASTM D638
Multibase Multi-Flex® A 5904 LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone Resistant Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Tensile Strength, Yield 7.58 MPa
1100 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7206 E TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Yield 7.58 MPa
1100 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 8502 A Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex APEX® 3300-45 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me..
Tensile Strength, Yield 7.58 MPa
1100 psi
100%; ASTM D412
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R..
Tensile Strength, Yield 7.58 MPa
1100 psi
100%; ASTM D412
Teknor Apex MF 569 Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex MONPRENE® MP 2780 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex TEKBOND® MP 1726 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex TEKBOND® MP 1726 UVF Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex TELCAR® 1050-75 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 7.58 MPa
1100 psi
Type 1, 20 in/min; ASTM D638
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex Vidux® CV-1000-91 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D412
Vicone High Performance Rubber VicoSeal™ 003R-BK High Performance EPDM Rubber
Two Material Product:Material 1: VicoSeal™ 003R-30 DUROMaterial 2: 11 ga CRS yellow anodized natural rubber vulcanized to yellow anodized steel (RoHS Approved)Information provided by Vicone
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D638-61T
Chevron Phillips 1018 Extrusion Coating Resin
Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Stability, Good Draw Down ResinApplications:Food Packaging, Laminations, Sealant ResinData provided by Chevron..
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D638-61T
Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin
Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che..
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D412
Teknor Apex APEX® 3200-45 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 7.60 - 12.0 MPa
1100 - 1740 psi
Average value: 9.81 MPa Grade Count:21
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Tensile Strength, Yield 7.58 - 17.9 MPa
1100 - 2600 psi
Average value: 11.3 MPa Grade Count:8
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min..
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D-638
Axiall 83-126K Moldings & Extrusions Flexible PVC
Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 7.60 MPa

@Strain 100 %
1100 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tensile Strength, Yield 7.58 MPa

@Strain 300 %
1100 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-4080 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma..