Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Techmer ES Electrablend® PC 04009 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF10 IM L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 NAT001 Nylon 6 Availability: North AmericaForms: PelletsFeatures: Good Processability and High FlowAppearance: NaturalTPCI# 1327102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Cheng Yu Plastic FV30G15 POM, 15% Glass Fiber |
|||
Tensile Strength, Yield | 74.5 MPa | 10800 psi | ASTM D638 |
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent
(discontinued **) Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009. |