Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ASTM D638 |
Nylene® 409 Nylon 6 Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527-1,2 |
Qualchem Danamid FEH Polyamide 6 Heat stabilized type polyamide, for long-lasting use at 120-130°CInformation provided by Qualchem Zrt. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527-1,2 |
Qualchem Danamid FEHUV Polyamide 6 Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial lightInformation provided by Qualchem Zrt. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/2 |
Radici Radiflam® SFR (dry) Nylon 6 PA6 Self-extinguishing without halogen or phosphorousInformation provided by Radici group. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Tensile Strength, Yield | >= 75.0 MPa | >= 10900 psi | |
MetalTek Bearium® B-4 Bearing Bronze Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mis.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | d.a.m.; ISO 527-1, -2; 50 mm/min |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-1/-2 |
Lanxess Durethan® B 40 E 000000 Nylon 6 PA 6 extrusion grade, standard grade of high viscosity with processing aid/lubricant, not nucleated. |
|||
Tensile Strength, Yield | 75.0 MPa @Temperature 22.0 °C |
10900 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527 type 1 A |
Solvay TECHNYL® C 230 PA6, DRY Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibili.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527 type 1 A |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific) PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66 Description: Dry impact unfilled Polyamide 6.6, good flowability and demolding properties.Application: Molding parts of different kinds, high impact properties.Information provided by Ter Hell Plas.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® FR 7067 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® FR 7087 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Makrolon® XT5010 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Easy processing• Low.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® EB 50 H PA6 Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImp.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6000 S Nylon 6, Finely Crystalline, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesti.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 90 TL PAMACM12 Product description: Grilamid TR 90 TL is a transparent thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic blocks. The special characteristic of Grilamid TR 90 TL is the high st.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ASTM D638 |
E-Polymers TEKAMID® TB120L Lubricated PA6, DAM LubricatedInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50mm/min; ISO 527-2 |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | |
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | ASTM value at 50 mm/min. |
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur.. |
|||
Tensile Strength, Yield | 75.0 - 110 MPa | 10900 - 16000 psi | Average value: 93.5 MPa Grade Count:6 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Yield | 75.0 MPa | 10900 psi | 50mm/min; ISO 527 |
BASF Ultrason S 6010 PSU Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (.. |
|||
Tensile Strength, Yield | 75.0 MPa @Strain 0.200 %, Temperature 1100 °C |
10900 psi @Strain 0.200 %, Temperature 2010 °F |
|
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°.. |